WELD TOE QUALITY GAUGES
To assure a high and even quality it is necessary to use gauges securing a repeatability of your procedures and a fulfillment of the specified requirements.
To remove potential defects at the weld toe we recommend a controlled undercut created with Micro-burr grinding and/or HFMI. The quality controll procedure is the following:
Visually inspect see that no defects are present in the undercut with help of a LED-torch.
Controll the undercut depth with our Depth gauge and backlight from the LED-torch. Recomended depth is 0.2 to 0.4 mm
Judge the radius of the undercut transition in the same way with our Radius Gauge. We recommend a radius larger than 1 mm for all procerures but for some applications it can be beneficial to use larger radiuses.
The only gauge you need to check a depth between 0.2 mm and 0.4mm, and a radius of 1.0, 1.5 or 2.0 mm. Suitable for both grinded and HFMI treated welds.
Article number: 1020
Price: 160 SEK
Depth gauge to judge the depth of a controlled undercut with a radius larger than 1 mm. With depth levels 0.2, 0.4, 0.6, 0.8 and 1.0 mm.
Article number: 1021
Price: 160 SEK
*Not suitable for fillet welds with a leg length smaller than 5-6 mm
Radius gauge to control the weld toe radius of butt and fillet welds. With Radius 1.0, 1.5, 2.0, 2.5 and 3.0 mm.
Article number: 1013
Price: 160 SEK
*Not suitable for fillet welds with a leg length smaller than 5-6 mm or with an undercut deeper than 1 mm
A quality gauge specially made for the Volvo Group standard 181-0004. With radius and angle levels according to the quality levels in the standard.
Article number: 1080
Price: 160 SEK
Please contact us for any enquiry!
Follow Weld-Hit on LinkedIN
Copyright © Weld-Hit AB -2023, All Rights Reserved
Weld-Hit AB, Rapphönsvägen 8, 363 31 Rottne, Sweden
Org nr: 559100-7777
VAT nr: SE559100777701
Godkänd för F-skatt
Key words: Fatigue life of welds, HFMI, UIT, Hammer Peening, Peening, Burr grinding, Post-weld- treatment, High frequency mechanical impact treatment, grinding of welds, fatigue life extension, TIG-treatment